| Item |
PN-1 |
PN-2 |
PN-3 |
PN-4 |
| Chemical Composition(%) |
AL2O3 |
20 |
30 |
30 |
30 |
| SiC |
25 |
25 |
30 |
35 |
| Si3N4 |
-- |
-- |
5 |
10 |
| Bulk Density(g/m3) |
2.10 |
2.20 |
2.30 |
2.30 |
| Linear Change(%) |
1300℃×3h |
±1.0 |
±1.0 |
±1.0 |
±1.0 |
| Modulus Rupture (Mpa) ≥ |
1300℃×3h |
2-5 |
2-5 |
2-5 |
2-5 |
| Cold Crushing Strength(Mpa) |
1300℃×3h |
6-12 |
6-12 |
6-15 |
6-15 |
| Volume of Furnace(m3) |
≦1000 |
1000-2000 |
2000-3200 |
≧2500 |
Note: According to the actual situation and user needs, the data in the table can be adjusted appropriately. Carbide Water-based Blast-furnace Plug Technical Index:
| Item |
Chemical Composition(%) |
| SiO2 |
AI2O3 |
ZrO2 |
MgO |
Fe2O3 |
fixed carbon |
loss on ignition |
| Property Value |
30-35 |
18-20 |
<0.5 |
>0.2 |
<2.5 |
35 |
40-45 |