| 项目 Item | 铬15刚玉砖 15 Chrome- Corundum Brick | 铬10刚玉砖 10 Chrome-Corundum Brick | 铬5刚玉砖 5 Chrome-Corundum Brick | 耐磨滑轨砖 Wear Resistance Skid Rail | 铝铬锆砖 Zr-Cr-Corundum Brick |
| Cr2O3(%) | ≥15 | ≥10 | ≥5 | ≥5 | ≥8 |
| Al2O3(%) | ≥75 | ≥80 | ≥85 | ≥85 | ≥60 |
| ZrO2 (%) | _ | _ | _ | _ | ≥15 |
| 显气孔率(%) Apparent Porosity | ≤18 | ≤18 | ≤18 | ≤16 | ≤18 |
| 体积密度(g/cm3) Bulk Density | ≥3.35 | ≥3.3 | ≥3.2 | ≥3.2 | ≥2.9 |
| 常温耐压强度(Mpa) Cold Crushing Strength | ≥120 | ≥120 | ≥120 | ≥130 | ≥90 |
| 荷重软化开始温度(℃) (0.2Mpa,0.6%) Refractoriness under Load | ≥1700 | ≥1700 | ≥1700 | ≥1700 | ≥1700 |
| 典型应用 Typical Application | 铬刚玉砖主要用于玻璃窑,炭黑炉,有色冶炼炉,垃圾焚烧炉,废酸处理炉,化工工业炉的内衬以及轧钢加热炉的滑道,出钢平台砖。 Mainly used for glass furance, carbon black furance, non-ferrous smelting furance, incinerator, chemical furance, waste acid treatment furance, as well as steel reheating furance skid rail, platform blocks. | ||||