| Item 项目 | Fireclay bricks for Hot Blast Stove 热风炉用粘土砖 | |||
| RN-42 | RN-40 | RN-36 | ||
| Al2O3(%) | ≥ | 42 | 40 | 36 |
| Apparent Porosity 显气孔率(%) | ≤ | 24 | 24 | 26 |
| Refractoriness 耐火度(℃) | ≥ | 1750 | 1730 | 1690 |
| Cold Crushing Strength 常温耐压强度(Mpa) | ≥ | 29.4 | 24.5 | 19.6 |
| Refractoriness under Load 荷重软化开始温度(℃) (0.2Mpa) | ≥ | 1400 | 1350 | 1300 |
| Reheating Linear Change Rate 重烧线变化(%) | 1400℃×2h | 0~0.4 | ____ | ____ |
| 1350℃×2h | ____ | 0~0.3 | 0~0.5 | |